A 10 mm × 10 mm × 100 mm alloy bar specimen was built by a L-PBF method from commercially available AlSi10Mg powder under Ar atmosphere using a Concept Laser M2 3D printer. Fig. 1(a) shows a schematic diagram of the utilized building strategy and specimen microstructure observed from th...
The algorithm for calculating the MCL for the multiple material phases requires the following four steps, a schematic diagram of which, is given in Fig. 4.12. 1. Arrange the j-material phases (j=1,…,NMP) in decreasing order of stiffness by using their Young’s moduli. The greatest value...
Finally, a diagram of a device that implements a capillary barrier discharge is shown in Figure 5 [158]. Figure 5. Capillary discharge device used for surface cleaning. Operating principle. A discharge implemented by a DBD source ignited at atmospheric pressure in a nitrogen working gas ...