4 that there were no remarkable differences between the surface morphologies of films made from nonmodified (BX) and those from carboxymethylated (CMBX) xylans, which was also shown by their root mean-squared roughness (Table 3). Obviously, in the case of CMBX, the majority of charge was dis...