Fiber-Reinforced Deck Mix is portland cement based, high-early strength 6000 psi concrete mixes. The fiber reinforce and air-entrained formula provide improved freeze/thaw durability and crack resist. Use For Balconies Roads Parking Structures Bridge Decks Available In 80lb bag View Spec Data Sheet...
3 hours 3000 psi (20.7 MPa) 24 hours 5000 psi (34.5 MPa) 7 days 6000 psi (41.3 MPa) 28 days 7000 psi (48.3 MPa) Slant shear bond strength, ASTM C928 1 day 1000 psi (6.9 MPa) 7 days 1500 psi (10.3 MPa) Shrinkage, ASTM C928 28...