When using PETG, try reducing the printing temperature in increments of 5 °C to see if stringing can be reduced without compromising print quality and durability, causing clogs, or negatively affecting adhesion (first layer or otherwise). You can also try increasing the cooling fan speed to coo...
Recalibrated 1st layer and used Overture PETG Black After full calibration, used Overture PETG White I performed full calibration between black and white Overture PETG filaments and things seemed to get worse, LOL. I am stuck and don't know what I should be ...
A lot of people seem to have problems with PETG in general, but it is in my experience very sensitive to moisture/humidity so that is the first thing to check Strange women, laying in ponds, distributing swords, is hardly a basis for a system of governa...
First layer height: 0.2mm Perimeter: 3 shells Top layers: 4 Bottom layers: 4 Overlap: 30% Infill: 25% Separation to model (raft): 0.2mm Cooling: On after 1st layer Extrusion multiplier: 1.1 Retraction distance 1.3 Retraction speed: 30mm/s Suggestions very much appreciated. RoboDLC Posts: ...
Once I've coated the bedplate for the first time, I'll let it air-dry and then apply a second layer going at right angles to the first, and then kick on the bed heater to set the product well.3. WAIT FOR THE BEDPLATE TO COOL DOWN before you remove the print! I wait for the...
You can just about make out the individual layers in the last photo (note that this is the "0.20mm Input Shaper" profile, but I changed the layer height to 0.3mm). I'm guessing this matt finish has something to do with the speed that the filament is...
The polymer foil industry is one of the leading producers of plastic waste. The development of new recycling methods for packaging products is one of the biggest demands in today’s engineering. The subject of this research was the melt processing of mul
Fair interlayer diffusion and a good diffusion between the pairs of deposited material for each layer height can be seen. This arrangement of pairs of the deposited material also confirmed visible air voids already detected by the XCT results. From the images, perceptible nucleation points and ...