Poor Bed Adhesion Problem: The first layer of the print doesn't stick to the bed, causing the print to fail. Solution: Ensure your print bed is level and the nozzle-to-bed distance is correctly set. Slightly increasing the first layer height can help with adhesion. Experiment with different...
First layer height: 0.2mm Perimeter: 3 shells Top layers: 4 Bottom layers: 4 Overlap: 30% Infill: 25% Separation to model (raft): 0.2mm Cooling: On after 1st layer Extrusion multiplier: 1.1 Retraction distance 1.3 Retraction speed: 30mm/s Suggestions very much appreciated. RoboDLC Posts: ...
Excellent first layer adhesion, improved adhesion between layers, reduced warping, shrinking, curling. Made from natural renewable resource, our filament is 100% biodegradable & non-toxic. COMPATIBILITY Our filament is compatible with nearly all 3D printers, including Ultimaker, MakerBot, Flashforge, ...
I haven't got a large bore nozzle yet but that should actually give even more transparent results when used in combination with a thick layer height. That should result in a smaller number of optical interfaces and thus give less blurring. jm0.0$ Hansjoerg ...
You can just about make out the individual layers in the last photo (note that this is the "0.20mm Input Shaper" profile, but I changed the layer height to 0.3mm). I'm guessing this matt finish has something to do with the speed that the filament is...
Additionally, this is the explanation of why the default increase in temperature settings is only applied during the first layer formation. This pattern was also valid for each other NT specimen printed with the 0.1 mm raster line. From Figure 5d–f, it can be seen that the measured ...
Keywords: fused deposition modeling (FDM); poly ethylene terephthalate glycol (PETG); resolution holes; printing speed; layer height; geometrical tolerance of hole's diameter; statistical analysis Citation: Alexopoulou, V.E.; Christodoulou, I.T.; Markopoulos, A.P. Effect of Printing Speed and ...
The variable parameters of FDM used in the manufacture of tensile and compression specimens from PETG and ASA are the height of the deposited layer in one pass, Lh = (0.10/0.15/0.20) mm and the filling percentage Id = (50/75/100)%. The mechanical properties of tensile (tensile strength,...
The polymer foil industry is one of the leading producers of plastic waste. The development of new recycling methods for packaging products is one of the biggest demands in today’s engineering. The subject of this research was the melt processing of mul