Therefore, the 7 5SrC3S-25HAp powder with 10 wt% of NaH2PO4 solution was mixed to prepare the slurry material. This slurry was measured for the working time and setting time at 37掳C under saturated vapor pressure. The material properties were evaluated in terms of crystal structures, surface...