The first stage was programmed from 30 ◦C to 200 ◦C at a heating rate of 10 ◦C min−1. This stage was applied to remove the previous thermal history which is particularly important in semicrystalline polymers. After this, a cooling stage from 200 ◦C down to 0 ◦C at a ...