The XRD pattern for the pellet after 2 days air exposure had a small peak at 2θ ~21.5°, which corresponds to the (110) reflections of Li2CO3 but was otherwise unchanged from the XRD pattern of the freshly polished sample. After the plasma treatment, the XRD results show that the LLZTO...