经第一次中子辐照得到氦含量为3mg/L和10mg/L的SS316LN-IG试样,为后面的实验做准备.随后,将末辐照与辐照后的SS316LN-IG相互组合,由钨极氩弧焊(TIG)焊接成3个试样.这些焊件在150℃,快中子注量约为7.5×10抖m.(E〉1MeV)的条件下进行再辐照.辐照后,分别在20℃和150℃的条件下,对焊件和母材进行拉伸试验...
SS316LN-IG specimens irradiated to helium contents of 3 and 10 appm He were prepared by the first neutron irradiation. Thereafter, the SS316LN-IG specimens with three different combinations of un-irradiation and irradiation were welded by a tungsten inert-gas (TIG) welding method. These ...
The International Journal of Advanced Manufacturing Technology -doi:10.1007/s00170-022-10154-xM. SulaimanY. H. ManurungB. ChangM. S. AdenanQairul Najmi EnseriN. MuhammadH. ChooM. F. MatB. AwiszusA. HaelsigSpringer LondonThe International Journal of Advanced Manufacturing Technology...
The wear characteristics of a laser cladded material were examined under dry sliding conditions, with sliding velocities ranging from 2.5 to 4.5m/s, loads varying from 10 to 40 N, and compositions of WC-NiCrBSi ranging from 15 to 60%. The worn surface was analyzed through SEM analysis to ...
Sulaiman, Mohd ShaharManurung, Yupiter H. P.Chang, BaohuaAdenan, Mohd ShahrimanEnseri, Qairul NajmiMuhammad, NorasiahChoo, Hui LengMat, Muhd FaizAwiszus, BirgitHaelsig, AndreSpringer LondonThe International Journal of Advanced Manufacturing Technology...