with process parameters: rotational speed 40 rpm, temperature 40–60 ◦C, mixing time 4 min, • dispersing fillers in plasticized natural rubber for 4 min in the same conditions, • introducing a weighed sulphur curing system for obtained mixtures on a two-roll mill at room temperature. ...