Pullout Performance of Fully and Partially Bonded Retrofit Anchors in Low Strength Concrete In the seismic retrofit of reinforced concrete structures, steel reinforcing bars are often used as post-installed chemical anchors to integrate new struct... T Gurbuz,A Ilki - 《Aci Structural Journal》 ...
The article does not include testing at temperature other than 23掳C, humidity, or moisture of the substrate.Daniel DudekMarta KadelaWorld multidisciplinary civil engineering-architecture-urban planning symposiumD. Dudek, M. Kadela, "Pull-out strength of resin anchors on non-and cracked concrete and...
CIP anchors of 10 ㎝ and 20 ㎝ embedment length in concrete with compressive strength of 280 kgf/㎠. Tested pullout capacities were compared to the ... YS Yoon,HS Kim,SY Kim - 《International Journal of Concrete Structures & Materials》 被引量: 2发表: 2001年 Tensile behavior of FRP an...
Parametric study of factors affecting the pull-out strength of steel rods bonded into precast concrete panels This paper deals with the effect of bond thickness, embedment length and type of epoxy adhesive formulation on the adhesion of steel anchors to concrete. T... A Çolak - 《...
Effects of chain pull-out on adhesion of elastomers Some theoretical considerations of fibre pull-out from an elastic matrix Pull-out strength of suture anchors for rotator cuff and Bankart lesion repairs A modified pull-out test for bond of near-surface mounted FRP rods in concrete ...
Nanotechnology-Based System for Damage-Resistant Concrete Pavements A scanning electron microscope was used to discern the difference between crack bridging and fiber pullout. Test results showed that the strength, ductility... Abu Al-Rub, R. K 被引量: 12发表: 2012年 The Development of Low-Cost...
In the lattice model used the heterogeneity of concrete is introduced by varying the strength or the length of the beam elements. To determine the strength values of each beam element, a generated grain structure is projected on top of a regular lattice. When heterogeneity is introduced by ...
17.Research on the pull strength of new concrete to old adherence with core-drilling and pull-stripping test新老混凝土黏结界面钻芯拉拔强度的试验研究 18.Pull-out model test for tunnel anchorage and numerical analysis隧道锚围岩拉拔模型试验研究及数值模拟 相关短句/例句 Pullout test拉拔试验 1.Developmen...
In the lattice model used the heterogeneity of concrete is introduced by varying the strength or the length of the beam elements. To determine the strength values of each beam element, a generated grain structure is projected on top of a regular lattice. When heterogeneity is introduced by ...
They observed that the pull-out strength of anchors below the critical depth of 6 was very close to the ones calculated by the Balla equation. They also observed, for shallow anchors with a H/B value less than 6, that an upheaval of the ground surface above the anchor was preceded by ...