THE MANUFACTURING PROPERTIES OF GALVANISED STEEL SHEET WITH HEXAGONAL AND TETRAGONAL NETWORK OF CIRCLE HOLESCircle holesmanufacturing propertiesstretchingdrawinggalvanized steelGalvanized steel sheet of 0.8 mm in thickness was drilled with circle holes of 2.5 mm diameter and spacing arranged in tetragonal and...
Similar and dissimilar combinations of a 1000 MPa galvanised dual phase (DP) steel, a 980 MPa transformation induced plasticity (TRIP) steel and a 980 MPa twinning induced plasticity (TWIP) steel were resistance spot welded under different welding parameters. The macrostructure, splash situation, nug...
The coefficient of static friction increased from 0.42 to 0.79, 0.39 to 0.75 and 0.36 to 0.69 for plywood, mild steel and galvanised iron, respectively. Bulk density increased with grain moisture content up to 10% and decreased with moisture content thereafter, while porosity decreased with ...
2023 Elsevier B.V.The present work investigated the resistance spot weldability of 0.85 mm thick galvanised CR210 steel sheets employing graphene nanoplate... T Das,SK Panda,KS Arora,... - 《Materials Chemistry & Physics》 被引量: 0发表: 2023年 Influence of resistance spot welding process par...
The static coefficient of friction of vetch seed increased the linearly against surfaces of four structural materials, namely, rubber (0·350–0·387), aluminium (0·319–0·367), stainless steel (0·202–0·328) and galvanised iron (0·312–0·361) as the moisture content increased from ...
The static coefficient of friction of spinach seed increased linearly against surfaces of four structural materials, namely, rubber (0.341 to 0.470), wood (0.318 to 0.391), stainless steel (0.271 to 0.364) and galvanised iron (0.321 to 0.388) as the moisture content increased from 11.93 to ...
The project is concerned primarily with the development of a process enabling hot dip galvanised (GI) or galvannealed (GA) steel to be produced using the same spelter chemistry, with the advantage that no zinc bath change or major compositional change is required (single-pot system). The secon...
The coefficient of static friction of the beans increased from 0.20 to 0.25, 0.45 to 0.60 and 0.53 to 0.7 for rubber, galvanised steel and plywood respectively. Introduction Cocoa (Theobroma cacao), believed to originate from the lower eastern equatorial slopes of the Andes is now grown mainly ...
The static coefficient of friction of black grape seed increased linearly against surfaces of four structural materials, namely, rubber (0.340 - 0.393), aluminium (0.196 - 0.270), stainless steel (0.247 - 0.337) and galvanised iron (0.322 - 0.397) as the moisture content increased from 8.26 -...
The static and dynamic coefficients of friction on various surfaces, namely, galvanised metal, chipboard, mild steel, plywood, and rubber also linearly increased with an increase in moisture content of each grain legume seed.Ebubekir Altuntas & Hilal Demirtola...