The wafer drying process was carried out for 30 s using N2 gas after the cleaning process was accomplished. The gate oxide was grown to 60 Å in a furnace to form an insulator (Figure 3d). The oxide thickness was measured by randomly selecting samples from among the produced wafers. The...