Afterwards, the PDA-treated cotton strips were immersed into the monomer solution for 30 min, followed by adding dropwise with the oxidant solution under stirring at 0 °C for 4 h. During the polymerization process, the color of the mixed solution turned from bright yellow to black. Fig. 1...