Description:PETGs (or copolyester) are glycol modified PETs; the modification is done by adding a second glycol during polymerization. The resulting molecular structure is irregular and the resin is clear and amorphous with a higher glass transition temperature of 88 C (190 F). PETGs can be pr...
If you want a glossy, glass-like finish, then you will have to use heated borosilicate glass printing bed. For a heated glass bed, we recommend a temperature of 50 to 60 °C. A thin layer of unscented hairspray will also improve adhesion. BuildTak printing surfaces also work very well ...
Thermal Resistance: Green PETG hasa high glass transition temperature (Tg) of approximately 80°C, indicating its ability to withstand elevated temperatures without losing its shape or properties. Transparency: Green PETG offers a high degree of transparency, allowing light to pass through it. This ...
Glass Transition Temperature (Tg) (DSC): 85°C Continuous Use Temp. (UL Yellow Card) (DSC): 50°C Recommended printing conditions: Nozzle Temperature: 200 - 250°C Print Bed Temperature: >60°C Fan Speed 0 - 50% Surface Adhesion Kapton, BigRep SWITCHPLATE Support Breakaway Specifications ...
Problem: Edges or corners of the print lift from the bed during printing, leading to a warped or curled print. Solution: Increase bed temperature to improve adhesion and minimize warping. Additionally, using a proper bed surface such as PEI, BuildTak, or glass can help with adhesion. Applying...
I also set up the glass bed and put down a layer of glue stick. No other changes to the setup. First thing I did was print another Benchy and there wasn't a noticeable change in quality. The first layer was more flat but there was still the same warping on the bow, ho...
If the PETG material still warps despite a leveled bed and increased bed temperature, it should be cleaned thoroughly. Different types of print beds require different approaches to cleaning. Glass plates should be thoroughly wiped with a streak-free glass cleaner and a clean cloth. PEI build ...
Glass transition temperature: 85 °C; Heat resistance: up to 75 °C. PETG has durability and impact resistance superior to PET. The material demonstrates good chemical resistance to both acidic and alkaline substances. It also has excellent moisture-blocking properties, which makes it suitable for...