Collections of free calculated patterns can be big. Their size only depends on the number of crystal structures. Special and user reference databases These databases are often small and contain measured pure substances or even phase mixtures. The HighScore software supports any number ...
Therefore, there is less SIM in WC than in CAC, as seen from the XRD results in Fig. S6. In the subsequent annealing process, the large-size deformed austenite grains are recrystallized to form large size fine grains. Dislocation cells and trace SIM are recrystallized into ultrafine grains. ...