The results show that microneedles produced from the nanocellulose loaded fish scale biopolymer requires higher temperature for micromolding (80 ± 5 °C) than microneedles from only fish scale biopolymer, which were moldable at 50 ± 5 °C. The mechanical properties of the fish scale biopolymer-...