2. Experimental Section The GO powder was prepared from graphite powder (particle diameter of 45 nm; 99.99%; Sigma-Aldrich, St. Louis, MO, USA) according to the modified Hummers method [34]. Then, the obtained GO powder (20 mg) was dispersed in deionized water (10 mL). The suspension...