(1) Chemical beneficiation: Mix potassium feldspar powder and alkali mother liquor at a ratio of 1kg:1.5~7.5L to make raw ore slurry. The raw ore slurry reacts at 200~300℃ for 5~240min, and the slurry is obtained after cooling. , filter to obtain desilica liquid and desilica concentr...