20 mg of each sample were weighted in an organic-cleaned steel cup (microscale precision: 0.01 mg) and place at the top of the pyrolyzer (cold). The cup was then lowered into the pyrolyzer’s oven heated at either 400 °C or 600 °C and stayed for 30 s at this tempera...