Glass substrates were cleaned sequentially with acetone, methanol, and isopropyl alcohol by sonication for 15 min before use. The composite solution was prepared by dissolving QDs and PMMA homopolymer (Mn = 60,000 g/mol) in toluene (0.5 wt% and 1 wt%, respectively). Then, thin fil...