After applying the coating, thermal curing, in a box oven at 175 ◦C for 15 min, was carried out to ensure proper adhesion onto the substrate. Thermal curing below 175 ◦C for 10 min resulted in a lower mobility of the PVDF containing droplets, preventing flow of the PVDF into the ...