网络铝脱氧钢;铝镇静钢 网络释义 1. 铝脱氧钢 Steelnet 华文专业钢铁网--产业辞典 ... 化学性质 CHEMICAL COMPOSITION铝脱氧钢AL-KILLED STEEL矽脱氧钢 SI-KILLE… www.steelnet.com.tw|基于6个网页 2. 铝镇静钢 配管工程术语及其缩写 - 豆丁网 ... air pocket 气袋Al-killed steel铝镇静钢alloy steel ...
测定了低碳铝镇静钢中氮化铝所含的氮。low carbon al-killed steel低碳铝镇静钢拼音 双语对照low carbon al-killed steel网络低碳铝镇静钢双语例句1Effect of continuous annealing process on mechanical properties of low carbon Al-killed steel sheet连续退火工艺对低碳铝镇静钢性能的影响
Steel sheet manufactured from Al-killed continuous cast carbon-manganese steel and having a hardness in the range 57 to 73 HR30T is characterized by a content of 0.03 to 0.10% by weight C and 0.15 to 0.50% by weight Mn, and an amount Z in ppm of dissolved uncombined nitrogen given by...
Based on the production practice oflow carbon low silicon Al-killed steelat JISCO,the mechanism of silicon picks up has analysised. 分析了低碳低硅铝镇静钢增硅的机理,结合酒钢CSP工艺实际,对增硅环节进行了改进和控制,使低碳低硅铝镇静钢:S i≤0。
1.Based on the production practice oflow carbon low silicon Al-killed steelat JISCO,the mechanism of silicon picks up has analysised.分析了低碳低硅铝镇静钢增硅的机理,结合酒钢CSP工艺实际,对增硅环节进行了改进和控制,使低碳低硅铝镇静钢:S i≤0。
This paper presents a new approach towards the evolution of non-metallic inclusion (NMI) populations in Ti-alloyed Al-killed steels, based on an extensive inclusion analysis campaign at Tata Steel Europe, IJmuiden Works. Automated SEM techniques were used to characterize the inclusion populations in...
The bake-hardenable cold-rolled steel sheets for the outer panels of auto-bodies exhibiting a sufficient formability and an excellent resistance to denting have been developed in box-annealing process. Examinations in the effects of chemical composition and box-annealing condition on the bakehardenabili...
A study is carried out to understand the CaS formation mechanism in an Al-killed high-S containing steel during the secondary refining process without a Ca-treatment. At the initial stage of the LF refining, CaS is formed on existing inclusions by the reaction between Ca and S due to the ...
We sampled the steel skull along the whole tundish bottom from under the ladle shroud (impact zone) up to the tundish well and nozzle. The microstructures imply that the steel solidifies to the refractory (gunning mass) and remains partially solid through the entire cast. Thus, a "mushy ...
Modification of MgO·Al2O3 spinel inclusions in Al-killed steel by Ca-treatment IeninaJonlMierl,ealrntratoluraofnasMtlgyaundMatraseil Voue1,mbr7Feray21Pae1 lm 8Nue ,bur01,g 8D0I1。 0,16 -1-340: 17s 10 09. 0O231 Moicto fg ? 23pie cuin -ie te yCatetetdfaino OA10 nlnlsos...