For the 3DP film deposition process illustrated in Figure 4b-top, the one-step solvent exchange process was used with the Lewis-base-acid adduct in 4:1 anhydrous DMF:DMSO with precursors MAI (1.5 M) and PbI2 (1.5 M), while the solution was stirred overnight at RT. Figure 4b-top ...