316 SS316 SUS316 Austenitic stainless steel sheet Length 2440mm,6000mm or according to your request Width 3mm-2000mm or as required Thickness 0.1mm-300mm or as required surface 2B,BA,NO1,NO4,NO8,mirror,etc Technique Hot rolled / cold rolled Surface Treatment 2B or according to customer...
Thermomechanical fatigue (TMF) studies were carried out on type 316 LN austenitic stainless steel (SS) base metal (BM) and its weld joint (WJ) with a tempe... TS Kumar,SD Yadav,A Nagesha,... - 《Materials Science & Engineering A Structural Materials Properties Misrostructure & Processing...
In this work, Plasma Nitriding was carried out at a temperature of 570掳C on nuclear grade austenitic stainless steel type AISI 316 LN (316LN SS) in a gas mixture of 20% N2鈥 80% H2 to improve the surface hardness and thereby sliding wear resistance. The Plasma Nitride (PN) treated ...
stainless steels (SDSSs), a sub-group of DSSs, have been developed recently withpitting resistance equivalentnumber (PREN) greater than 40 and excellent mechanical properties. Nevertheless, DSSs and SDSSs are susceptible to sensitization at 600 to 950°C arising from the precipitation of the Cr-...
Austenitic Stainless Steel Austenitic stainless steel is a type of stainless steel that is widely used in various industrial applications due to its excellent corrosion resistance and versatility. Austenitic stainless steels are versatile and popular materials, known for their corrosion resistance, high-...
S. Matsuoka, Relationship Between 0.2% Proof Stress and Vickers Hardness of Work-Hardened Low Carbon Austenitic Stainless Steel, 316SS, Jpn. Soc. Mech. ... N Nagashima,S Matsuoka - 《Journal of the Japan Institute of Metals》 被引量: 22发表: 2005年 The effects of grain and specimen sizes...
It was observed that the variation in values of n and K are associated with the precipitation of the different micro-alloyed elements presented in the stainless steel SS316L. It can be also concluded that the texture plays an important role in the resulting kinetics change....
This paper reports the effect of process parameters such as voltage, wire feed rate and shielding gas flow rate on the amount and composition of respirable welding fumes generated in the breathing zone of a welder during the Flux Core Arc Welding (FCAW) of austenitic stainless steel, SS-316LN...
The chemical composition of the baseline material is presented in Table 3, as AFA-SS 1. This alloy has already been reported to form alumina scale after oxidation at 800 °C for 72 h [6], and is one of the first successful alumina-forming stainless steels. This alloy, in addition, has...
A comparison has been made between the mechanical properties and swelling of austenitic stainless steels EP-838 (Fe-Cr-Mn) and 316SS (Fe-Cr-Ni) irradiated in the mixed-neutron spectrum of the SM-2 reactor in the temperature range 400–800°C (every 100°C) to 16 dpa dose with 1000 ...